Tabarak Marble Logo
Red Aswan

Red Aswan

TestMethodResult
1Determination of water absorption at atmospheric pressure0.70 %
2Determination of modulus of rupture 16.2 N/mm ²
3Determination of flexural strength 15.3 N/mm ²
4Determination of compressive strength155.8 N/mm ²
5Determination of Abrasion Resistance 31.2 HA
6Determination of apparent real density2615 KG/m ³