Galala Cream

TestMethodResult
1Compressive Strength (ASTM C 170)10300 psi
2Flexural Strength (ASTM C 880)1200 psi
3Abrasion Resistance (ASTM C 241/ C 1353)40.1 Ha
4Density (ASTM C 97) 2561
5Water Absorption (ASTM C 97)1.42%
6Modulus of Rupture (ASTM C 99)1700 psi